Glass fiber reinforced ABS is made by mixing, extruding, and cutting ABS resin and glass fiber. Mainly using injection molding method to form products, glass fiber reinforced ABS improves the thermal deformation temperature and mechanical properties of ABS, reduces the molding shrinkage rate and linear expansion coefficient. Used for manufacturing products with high dimensional accuracy requirements.
Contact NowABS-GF
ForceTracer™ ABS-GF is an acrylonitrile-butadiene-styrene (ABS) material with added chopped glass fibers. The long-term use temperature can reach 80 ℃, with high cost performance and high mechanical properties. It is mainly used in many professional scenarios such as normal temperature molds and automobiles .
ABS-GF 3D printing performance parameters
performance Property | numerical value Parameter Value | unit Unit | Test Methods Test Method |
Young's modulus/Tensile modulus | 3198 | MPa | ISO 527, Type 1A |
Tensile strength/Tensile strength | 84 | MPa | ISO 527, Type 1A |
Elongation at break/Elongation at break | 7 | % | ISO 527, Type 1A |
Bend modulus/Bend modulus | 3980 | MPa | ISO 14125 |
Bend strength | 110 | MPa | ISO 14125 |
Notched impact strength/Notched impact strength | 7 | kJ/m2 | ISO 180 |
Heat distortion temperature/HDT | 94 | ℃ | ISO 75-1,2 |
Particle printing temperature: from feed to nozzle 190-220 ℃, adding cavity temperature (90~110 ℃) will give better printing effect.
Drying temperature: 80℃ 4-6h